In Germany, expenditure for the construction of new and maintenance of existing federal highways is currently at a record level of EUR 8 billion per year. In connection with the planned infrastructure policy reforms it is necessary to further develop the planning tools for dimensioning and substance assessment of road structures in order to increase the efficiency of construction measures. The stress caused by traffic is of central importance here. Since unevenness in the road surface has a significant influence on the dynamic part of the wheel load, dynamic effects must be explicitly taken into account. As a result, increasing unevenness can lead to higher dynamic loads and, in the context of a corresponding number of wheel rollovers, to disproportionate damage to the road structure. In general, a shock factor is taken into account during dimensioning, which is to be considered as a function of vehicle suspension, load, speed and evenness. This approach is not sufficient for concrete road structures executed as slabs. In the normal case, only the periodically occurring individual event of a transverse contraction joint, superimposed by irreversible and/or temporary slab deformations, can lead to a significant increase in the dynamic wheel load. In addition, the existing slab deformations are tied to many boundary conditions and can therefore vary greatly in their characteristics. For the further development of methods for dimensioning and residual substance assessment with regard to their accuracy, a three-dimensional slab-specific view of the road surface is therefore appropriate. In this paper, a suitable measuring method for three-dimensional surface laser scanning and an algorithm for the classification of slab deformations are presented.
Für die rechnerische Dimensionierung der Betondecken im Oberbau von Verkehrsflächen für den Neubau sowie die Erneuerung nach RDO-Beton 09 ist die statische Spaltzugfestigkeit an der unteren beziehungsweise unteren und oberen Scheibe des Betonzylinders beziehungsweise Bohrkerns entsprechend der Vorgaben der AL Sp-Beton zu bestimmen. Aufgrund der unzureichenden Kenntnis der Präzision dieses Prüfverfahrens wurden mit einem breit aufgestellten Ringversuch die statistischen Kennwerte an Labor- und Bestandsbetonen unter Vergleichs- und Wiederholbedingungen auf der Grundlage des FGSV-Merkblatts über die statistische Auswertung von Prüfergebnissen ermittelt. Für eine möglichst gute statistische Absicherung nahmen an dem Ringversuch dreizehn erfahrene Prüfstellen teil. Zur Abdeckung des vielschichtigen Einsatzes des Prüfverfahrens erfolgte der Ringversuch an acht Prüflosen. Dabei berücksichtigen einerseits die Prüflose 1 und 2 mit den im Transportbetonwerk hergestellten Betonzylindern die Erst-/Eignungsprüfung und das darauf aufbauende Prüflos 3 mit Bohrkernen aus einer im Feldversuch hergestellten Fahrbahnplatte mit gleicher Betonrezeptur die Übereinstimmungskontrolle bei Neubaumaßnahmen. Andererseits findet der Einsatz des Prüfverfahrens bei der Restsubstanzbewertung von Betonfahrbahnplatten bei den Prüflosen 4 bis 7 mit den Bohrkernen aus vier in Waschbetonbauweise ausgeführten Fahrbahnplatten Berücksichtigung. Das zusätzlich aufgenommene Prüflos 8 mit einem Labormörtel dient der Herausarbeitung des Materialeinflusses auf die Präzision der Spaltzugfestigkeitsprüfung. Zusammenfassend kann festgestellt werden, dass die Präzision der in der AL Sp-Beton beschriebenen Spaltzugfestigkeitsprüfung mit einem Variationskoeffizienten von weniger als 10 % unter Wiederhol- und Vergleichsbedingungen hinreichend genau ist. Der geringe Unterschied zwischen den Variationskoeffizienten unter Wiederhol- und Vergleichsbedingungen lässt zusätzlich den Schluss zu, dass der Einfluss des unterschiedlichen Personals und der verschiedenartigen Prüftechniken bei den einzelnen Prüfstellen relativ gering ist. Die im Rahmen des Ringversuchs gewonnenen Erkenntnisse haben bereits partiell Eingang in die Normung gefunden.
Mit Hilfe der Datenbestände von 7 Städten werden die Grundlagen für eine praxisgerechte Weiterentwicklung des Bewertungsverfahrens für den messtechnisch erfassten Zustand von Innerortsstraßen mit den erforderlichen Normierungsfunktionen, den Ziel-, Warn- und Schwellenwerten und maßgeblichen Funktionsklassen erarbeitet. Für die Auswerteabschnitte ergab sich eine Länge von 10 m als sinnvoll, aus der problemlos Zustandsindikatoren auch für längere Abschnitte ermittelt werden können. Die bisher verwendeten Zustandsindikatoren für die Längsebenheit, Querebenheit und Substanz werden auf ihre Brauchbarkeit untersucht und verbesserte beziehungsweise neue Indikatoren mit den dazugehörigen Normierungsfunktionen vorgeschlagen. Für die Griffigkeit standen keine Analysedaten zur Verfügung. Hier konnte für die Festlegung von Ziel-, Warn- und Schwellenwerten auf entsprechende Normierungsfunktionen für Außerortsstraßen zurückgegriffen werden. Weiterhin werden Vorschläge für die Verknüpfung zum Gebrauchs-und Substanzwert erarbeitet. Für die Relativierung der Anforderungen an den Zustand von Asphaltfahrbahnen werden zwei Funktionsklassen für die Straßenkategorien "Hauptverkehrs-/verkehrs-/Sammelstraßen" (FK 1) und "Anlieger-/Wohnstraßen" (FK 2) vorgeschlagen. Weiterhin wird eine dritte Funktionsklasse für Pflasterstraßen eingeführt. Ihre unterschiedlichen Normierungsfunktionen gewährleisten bei gleichen Zustandsausprägungen eine unterschiedliche Einstufung der Dringlichkeit von Maßnahmearten. Die Untersuchungsergebnisse sind zusätzlich in Form eines Arbeitspapiers aufbereitet.
Annual report 2018
(2019)
With this annual report, BASt is giving the 2018 research year a face. A part of its work is present and in the focus of the public, for example the field test of long trucks, the unique research area duraBASt at the motorway junction Cologne East or the innovative measuring vehicle MESAS for the condition assessment of road surfaces in flowing traffic. A large part of the BASt's work is less effective in attracting public attention but no less important, such as the essential updating of regulations, the testing and approval of products and processes, and the compilation of forecasts and statistics. More than 50 employees report on their research activities and thus give an insight into the tasks of BASt with its core areas of vehicle technology, traffic safety, traffic engineering, road construction as well as bridge and civil engineering. Highlights as well as facts and figures in short and concise form complete the report.
Betonfahrbahndecken können grundsätzlich in zwei Varianten ausgeführt werden: unbewehrt und bewehrt. In Deutschland ist die unbewehrte Plattenbauweise mit verdübelten Querscheinfugen im Abstand von 5 m bis heute die Standardbetonbauweise. Die Nutzungsdauer wird in den RStO mit 30 Jahren angegeben. In anderen Ländern, wie Belgien und USA, wird die Durchgehend Bewehrte Betonfahrbahndecke (DBBD) standardisiert ausgeführt. Bei dieser Bauweise werden keine Querfugen in der Betondecke hergestellt, sondern es stellt sich ein freies Rissbild mit schmalen Plattenstreifen ein. Um eine Querkraftübertragung zu sichern, wird die Riss - öffnungsweite durch die Anordnung einer durchgehenden Längsbewehrung beschränkt. Bei dieser Bauweise ist eine Nutzungsdauer von mehr als 30 Jahren vorgesehen. Beide Bauweisen können dünnschichtig überbaut werden und es entsteht die Kompositbauweise. Dies kann im Neuzustand erfolgen oder als Erhaltungsmaßnahme. Als Beläge sind Splittmastixasphalt (SMA), Offenporiger Asphalt (OPA), Dünnschichtkaltbelag (DSK) u. a. möglich. Bei der Plattenbauweise sind dann im Fugenbereich zusätzliche Maßnahmen erforderlich. Im Falle DBBD entfällt dies. Zur Sammlung erster Erfahrungen in Deutschland wurden zwei Versuchsstrecken in DBBD angelegt und zwei Strecken mit SMA überbaut, davon eine in Plattenbauweise und eine in DBBD. Über die dabei gewonnenen Erfahrungen wird berichtet und ein Konzept für die weitere Erprobung der Kompositbauweise wird dargestellt.
Mobility is a central requirement for economic growth, employment and participation of each individual in social life. This basic principle of the BMVI (Federal Ministry of Transport and Digital Infrastructure) requires an intact and functional infrastructure. In a context of increasing investments over the next few years, it will be relevant to develop a network related systematic procedure to be part of the structural maintenance of the federal highway network. In the planning of maintenance measures, the knowledge about the state of structural performance and its long-term development is of central importance. In the following, a method is presented which allows the mechanically and statistically reliable assessment and prognosis of structural performance of concrete pavements. In addition, the application and procedure are applied to a case study.
Bau und Messungen an einer Versuchsstrecke mit optimierter Kiestragschicht unter der Betondecke
(2018)
Im Rahmen des Forschungsvorhabens wurde ein bereits unter Laborbedingungen bewährtes Baustoffgemisch 0/32 mm " bestehend aus gebrochenen und ungebrochenen Gesteinskörnungen - für die Herstellung einer modifizierten Kiestragschicht unter einem Betonfahrbahndeckensystem einer realen Versuchstrecke verwendet. Die messtechnische Begleitung dieses Versuchsstreckenbaus an einer Fahrgasse der Tank- und Rastanlage Köschinger Forst (BAB 9) im Sommer / Herbst 2012 umfasste unter anderem umfangreiche Tragfähigkeitsmessungen auf den einzelnen ungebundenen Schichten des Oberbaus. Die 30 cm dicke modifizierte Kiestragschicht wurde mit einer 27 cm dicken unbewehrten Betonfahrbahndecke in Plattenbauweise überbaut. Die Tragfähigkeitsmessungen auf der modifizierten Kiestragschicht wurden unmittelbar nach dem Einbau und nach 16 Tagen unter freier Witterung und Baustellenverkehr durchgeführt. Bei allen Messungen wurden die Vorgaben der ZTV SoB-StB " Ev2 ≥ 150 MPa " erfüllt. Eine Fuge der Fahrgasse wurde unverdübelt und ohne Fugenmasse ausgeführt, um durch die erhöhten Relativbewegungen der Plattenränder und den gleichzeitigen hohen Wassereintrag eine Erosion der Tragschicht im Fugenbereich zu induzieren. Im Mai 2015 erfolgten - nach 32-monatiger Liegedauer - die Wiederholungsmessungen. Die Überrollungen der unverdübelten Querscheinfuge konnten zum damaligen Zeitpunkt grob mit 350.000 Fahrzeugen (ca. 1 Mio. äquivalente 10t-Achsen) abgeschätzt werden. Für die Wiederholungsmessungen wurden zwei Einzelfahrbahnplatten der Lkw-Fahrgasse abgehoben. Es konnten hierbei keine wesentlichen Veränderungen der für eine KTSuB relevanten Performanceparameter festgestellt werden. Die in den ZTV SoB-StB und den RStO geforderten Mindestwerte der Tragfähigkeit - statischer Verformungsmodul und Verhältniswert Ev2/Ev1 - konnten an allen untersuchten Prüfpunkten eingehalten werden. Des Weiteren konnten die Bedenken hinsichtlich der Erosions- und Umlagerungsbeständigkeit im Fugenbereich beim vorliegenden - relativ langsam fahrenden Schwerlastverkehr - relativiert werden.
Bei der Herstellung von Betonfahrbahndecken kommen in Deutschland vorzugsweise Portlandzemente zur Anwendung, da mit dieser Zementart hinreichende Erfahrungen vorliegen. In vielen Bereichen des Betonbaus werden jedoch seit einigen Jahren zunehmend CEM II- und CEM III-Zemente verwendet. Durch den gezielten Einsatz von CEM II- und CEM III-Zementen im Betonstraßenbau lässt sich zum Beispiel die Ökologie des Bauwerks "Betonstraße" verbessern, da unter anderem bei der Herstellung dieser Zemente vergleichsweise weniger CO2 emittiert wird. Um diesen Vorteil nutzen zu können, sollte eine allgemeine Erfahrungssammlung erstellt werden. Hierfür wurden die im bundesdeutschen Fernstraßennetz befindlichen Betonfahrbahndecken mit CEM II- und CEM III-Zementen ermittelt sowie deren Oberflächensubstanz begutachtet und bewertet. Bis dato konnte festgestellt werden, dass diese im Vergleich zu den CEM I-Betonen Auffälligkeiten an der Betonoberfläche aufweisen können. Ferner wurde auf Verkehrsflächen aus CEM II-Beton nach sehr langer Nutzungsdauer ein Gebrauchs- beziehungsweise Substanzwert kleiner 1,5 ermittelt.
Im Jahr 1981 wurde die erste Versuchsstrecke mit einer Betondecke auf einer Tragschicht mit hydraulischem Bindemittel und einer Vliesstoffzwischenschicht hergestellt. Es zeigte sich, dass bei dieser Bauweise Probleme in Form von Plattenpumpen und Erosionen nicht auftreten. Im Rahmen von mehreren Erprobungsstrecken wurde das positive Verhalten bestätigt. Im Jahr 2001 wurden die Bauweise mit Vliesstoffzwischenschicht als eine neue Standardbauweise eingeführt und Anforderungen an die Verlegung der Vliesstoffe und die zu verwendenden Produkte festgeschrieben. Im Weiteren erkannte man, dass neben der Anwendung bei Neubaumaßnahmen der Vliesstoff auch bei der Überbauung von schadhaften Betondecken sinnvoll eingesetzt werden kann. Trotz der guten Erfahrungen blieb die Bauweise aber über Jahre eine deutsche Besonderheit, bis im Jahr 2006 eine amerikanische Delegation die Bundesanstalt für Straßenwesen besuchte und sich über Innovationen im Straßenbau informierte. Dabei wurde auch die Bauweise mit Vliesstoff vorgestellt. Man erkannte das Potenzial dieser Bauweise und im Jahr 2008 wurden zwei Versuchsstrecken mit Betondecken auf Vliesstoff in den amerikanischen Bundesstaaten Missouri und Oklahoma eingerichtet.
In der Vergangenheit stiegen die Verkehrsbelastung und der Anteil des Schwerverkehrs auf deutschen Straßen und Autobahnen nahezu stetig. Dies wird sich auch in der Zukunft fortsetzen. Um auch zukünftig Mobilität gewährleisten zu können, sind Bauweisen mit maximaler Nutzungsdauer und minimalen Erhaltungsaufwendungen erforderlich. In Deutschland werden Betonfahrbahndecken als unbewehrte direkt befahrene Betonfahrbahnplatten mit Querfugen in regelmäßigen Abständen gefertigt und für Nutzungsdauern von 30 Jahren konzipiert. Die Querfugen stellen dabei den schwächsten Bereich in der Konstruktion dar. Betonfahrbahndecken können auch als Durchgehend Bewehrte Betonfahrbahndecke gefertigt werden. Dabei stellt sich ein freies Rissbild mit schmalen Plattenstreifen ein. Um eine Querkraftübertragung zu sichern, wird die Rissöffnungsweite durch die Anordnung einer durchgehenden Längsbewehrung beschränkt. Die Erfahrungen zeigen, dass mit dieser Bauweise eine längere Nutzungsdauer und ein höherer Fahrkomfort erreicht werden und weniger Erhaltungsmaßnahmen erforderlich sind. Durchgehend Bewehrte Betondecken eignen sich besonders gut für eine Asphaltüberbauung, da es keine Querfugen als Störstellen gibt. Diese Komposition hat das Potenzial für eine Nutzungsdauer von 50 Jahren und erfordert geringere Kosten, wenn man den gesamten Lebenszyklus betrachtet. Um baupraktische Erfahrungen zu sammeln, wurde im Jahr 2011 auf der Bundesautobahn (BAB) A 94 bei Forstinning in Bayern eine Versuchsstrecke eingerichtet. Diese besteht aus drei Abschnitten von je etwa 4 km Länge: Durchgehend Bewehrte Betondecke mit DSH-V-Überbauung, unbewehrte Betondecke in Plattenbauweise mit DSH-V-Überbauung und unbewehrte Betondecke in Plattenbauweise mit Grinding-Oberfläche. Erste Ergebnisse bezüglich Rissbildung, Bewegungen an den Endspornen, Haftverhalten des Blacktopping und der Schallmessungen liegen vor.
Bewertung der strukturellen Substanz für die systematische Erhaltungsplanung von Betonfahrbahndecken
(2016)
"Mobilität ist zentrale Voraussetzung für wirtschaftliches Wachstum, Beschäftigung und Teilhabe des Einzelnen am gesellschaftlichen Leben." Dieser Leitsatz des BMVI setzt eine intakte und funktionierende Infrastruktur voraus. Im Kontext mit dem Investitionshochlauf in den nächsten Jahren ist für das Bundesfernstraßennetz insbesondere ein netzbezogenes systematisches Vorgehen im Rahmen der Baulichen Erhaltung von Relevanz. Bei der Planung von Erneuerungsmaßnahmen ist dabei die Kenntnis über den Zustand der strukturellen Substanz und deren langfristige Entwicklung von zentraler Bedeutung. Nachfolgend wird ein Verfahren vorgestellt, das die mechanisch und statistisch abgesicherte Bewertung und Prognose der strukturellen Substanz von Betonfahrbahndecken ermöglicht. Zudem werden die Anwendung und das Vorgehen anhand eines Praxisbeispiels aufgezeigt.
Das Forschungsvorhaben verfolgte das Ziel, die Applikation der Oberflächenhydrophobierung bei Betonfahrbahndecken zu optimieren und deren Einfluss auf die schädigende AKR zu bewerten. Die Literaturrecherche zum Stand der Technik ergab, dass bisher primär Silane zur Hydrophobierung von Betonen mit erhöhtem AKR-Schädigungspotenzial im Betonstraßenbau mit unterschiedlichem Erfolg Anwendung fanden. National beschränken sich die Erfahrungen auf den praktischen Einsatz von WA65 auf wenige BAB-Abschnitte (A 9 und A 14). Wissenschaftliche Untersuchungen hierzu fehlen. Vor diesem Hintergrund erfolgten umfangreiche Laboruntersuchungen am Bestands- und Laborbeton zur: - Optimierung der Applikation des Hydrophobierungsmittels, - Bewertung der Dauerhaftigkeit der hydrophobierten Betonrandzone, - Analyse der Auswirkungen der Oberflächenhydrophobierung auf den AKR-Schädigungsprozess. Als Hydrophobierungsmittel kamen die auf dem Wirkstoff Oktyltriethoxysilan basierenden Produkte WA65 und LM7 als Emulsion und GEL30 (Acrylatgel) zum Einsatz. Ihr Verhalten im neu entwickelten Applikationstest war beim Bestandsbeton deutlich schlechter als beim Laborbeton. Hier erwiesen sich WA65 und LM7 als gleichwertig brauchbar, während die geprüfte Modifikation des GEL30 aufgrund seiner geringen Eindringtiefe abzulehnen ist. Bei den aufbauenden Untersuchungen wurden folgende Erkenntnisse gewonnen: - Nachweis der Dauerhaftigkeit der hydrophobierten Betonrandzone im zyklischen Schwingversuch mit aufstehender Prüflösung (exemplarischer Test mit WA65), - Nachweis der Verminderung des AKR-Schädigungsprozesses durch Applikation von WA65 bzw. LM7 auf Bestands- und Laborbeton mittels Klimawechsellagerung (Beaufschlagung mit NaCl-Lösung). Mit einem Langzeitmonitoring des Feuchte- und Salzhaushalts in ausgelagerten Ausbausegmenten mit unterschiedlicher Schadensausprägung im Bereich der Querscheinfuge wird langfristig die dortige Gefahr der Hinterläufigkeit der hydrophobierten Betonrandzone untersucht und bewertet.
As investigations by BASt have shown, a bond between concrete surfaces and bases may be a disadvantage when water penetrates via joints and from the sides if the bond becomes partially detached at an early stage. Free water may penetrate into the area between the concrete surface and the base and build up in areas where the bond is still intact. The high pressure caused by lorry wheels rolling over the pavement causes hydrodynamic pumping. This creates very high flow speeds with considerable corrosion power. This results in the base course surface being eroded in the areas where heavy vehicles drive over the road and may even lead to water and fine particles from the base courses being expelled through the longitudinal joints between the pavement slab and the lower hard shoulder or first overtaking lane. The erosion of the base leads unavoidably to the bearing conditions deteriorating and increased loading of the concrete surface. Cracks may occur and, later stepping-off and tilting of the plates components. This significantly deteriorates the evenness and consequently the service value of the road. This finally leads to a reduction in the service life of the concrete surface. To avoid such damage water which has penetrated must be able to lose pressure and to then seep away. A possible solution is: A nonwoven fabric substance between concrete suface and bound base course. This construction method has proved himselve on numerous test road sections and were rightly included in the new Codes of Practice for the Standardisation of the Upper Structure of Traffic-Bearing Surfaces (Richtlinien für die Standardisierung des Oberbaues von Verkehrsflächen- RStO).
Für die Herstellung von Betonfahrbahndecken ist für Ober- und Unterbeton ein Zement der gleichen Art und Festigkeitsklasse zu verwenden. Durch eine flexiblere Handhabung von Bindemitteln im Ober- und Unterbeton können sich ökologische und wirtschaftliche Vorteile eröffnen. Ein sinnvoller Ansatz ist die Verwendung von Zementen mit hohem Klinkeranteil für den hochbelasteten, dünnen Oberbeton in Verbindung mit Zementen mit reduziertem Klinkeranteil für den Unterbeton. So kann die Ökobilanz der Betonstraße verbessert und die Gefahr einer schädigenden Alkali-Kieselsäure-Reaktion (AKR) im Unterbeton vermindert werden. Vorteile können sich ebenfalls aus einem teilweisen Zementersatz durch Steinkohlenflugasche im Ober- sowie Unterbeton ergeben. Da die Anrechnung der Flugasche auf den Wasser/Zement-Wert des Fahrbahndeckenbetons nicht gestattet ist, wird Flugasche in der Regel nicht für den Bau von Verkehrsflächen aus Beton verwendet. Im Rahmen des Forschungsvorhabens sollten die notwendigen betontechnologischen Kenntnisse gewonnen werden, um eine kritische Bewertung der genannten Einschränkungen in der Bindemittelanwendung im Betonstraßenbau vornehmen zu können. Im Ergebnis wurde eine Modifizierung der Einschränkungen angestrebt. Es galt nachzuweisen, dass sich unter den spezifischen Randbedingungen von Fahrbahndecken aus Beton weder für Herstellung, Nutzung sowie Dauerhaftigkeit (insbesondere Frost-Taumitteleinwirkung) Nachteile oder Beeinträchtigungen ergeben. Insbesondere war dabei das Verbund- und Verformungsverhalten von Ober- und Unterbeton zu berücksichtigen. Weiterhin wurde untersucht, inwiefern durch die Verwendung von hüttensandhaltigen Zementen bzw. von Flugasche im Unterbeton das Risiko einer AKR vermindert wird und dadurch die Anzahl an verwendbaren Gesteinskörnungen im Unterbeton vergrößert werden kann. Aus labortechnischer Sicht sowie auf Basis theoretischer Betrachtungen wurden die angestrebten Vorteile der Verwendung unterschiedlicher Bindemittel in Ober- und Unterbeton bei vertretbaren technologischen Risiken erzielt. Insbesondere das AKR-Schadenspotential ausgewählter kritischer Gesteinskörnungen konnte durch Einsatz hüttensandhaltiger Zemente sowie auch durch Steinkohlenflugasche deutlich gesenkt werden. Die Anrechnung von Steinkohlenflugasche auf w/z-Wert und Zementgehalt verursachte in Verbindung mit klinkerreichen Zementen (bis 15 % HÜS) keine nennenswerte Verminderung des Frost-Tausalz-Widerstandes. Auf Grundlage der gewonnenen Erkenntnisse kann die Beachtung der aufgezeigten Ansätze im Regelwerk empfohlen werden. Eine baupraktische Bestätigung dieser Ergebnisse, z. B. in Form einer Probestrecke ist zu empfehlen.
Knowledge of material properties is of great importance when developing new types of concrete and construction methods for road building, and for quality control and quality assurance. Physical material characteristics are likewise the basis for dimensioning and assessing the residual substance of concrete pavements. One relevant characteristic when examining thermally induced stress and deformation is the coefficient of thermal expansion (CTE) of concrete. This indicator, for example, significantly influences the longitudinal expansion of the pavement system as well as the degree of curling of slabs and joint movements. Extensive tests were conducted during the technical engineering assessment of the structural substance of concrete pavements in the German motorway network, including tests to determine the CTE of existing types of concrete. Because no standardised procedure currently exists in Germany for using tests to determine the CTE of concrete, the initial task was to develop a suitable test procedure from a road-building perspective, taking consideration of the national prevailing structural conditions. This article presents the results of selected status analyses, in which the CTE was determined for a total of 656 individual samples. The values calculated for the top and bottom drilled core layer are in the range 8.9 – 13.2 x 10-6/K, whereby the average CTE assumes a value of 10.7 x 10-6/K. The deviations of the CTEs from the bottom and top drilled core layer are in principle significantly below the limitation to a maximum of 2.50 x 10-6/K recommended in literature.
Betondecken auf Schottertragschichten sind bewährte Bauweisen. Bei der Anwendung von Schottertragschichten unter Betondecken (STSuB) werden besondere Anforderungen nach TL/ ZTV SoB-StB 04 gestellt. Ob mit Kiestragschichten mit optimiertem Anteil gebrochener Gesteinskörnung die geforderte Umlagerungs- und Erosionsbeständigkeit unter Betondecken erreicht werden kann, wurde an 5 Varianten einer Tragschicht ohne Bindemittel (ToB) untersucht (2 STSuB, 1 Kiestragschicht (KTS), 2 modifizierte Kiestragschichten). Die Anforderungen an die bodenmechanischen Kennwerte (Korngrößenverteilung, Proctordichte, CBR-Wert, Wasserdurchlässigkeit) wurden in der Regel eingehalten. Dauerschwellversuche mit Lastplatte auf ToB, die schweren Baustellenverkehr simulieren sollen, zeigen eine Zunahme der plastischen Verformung der ToB mit dem Logarithmus der Lastwechselzahl, womit eine vergleichende Bewertung ermöglicht wird. Beim Dauerschwingversuch im Großprüfstand mit Betonplatte mit Fuge auf ToB wurde die Belastung der Fugenränder und die Phasenverschiebung so eingestellt, dass die Überfahrt eines schweren Lkw über die Fuge mit stufenweiser Zunahme der Schwingweite in 4 Versuchsphasen simuliert wird. Die gezielte Wasserzugabe über die Fuge führte zu einer starken Zunahme der bleibenden Verformung. Die größere Einsenkung und bleibende Einsenkung am "zuletzt befahrenen" Fugenrand steht in Übereinstimmung mit den Beobachtungen der Stufenbildung in situ (in Fahrtrichtung abwärts), ebenso ein stärkeres Freilegen der groben Gesteinskörnung an der Oberseite infolge Pumpens. Eine Feinkornumlagerung an die Unterseite der ToB konnte aus der Korngrößenverteilung nicht abgelesen werden. Eine tendenzielle Veränderung der Wasserdurchlässigkeit vor und nach dem Dauerschwingversuch war nicht festzustellen. Bei der Versuchsreihe war der CBR-Wert kein geeignetes Kriterium für die Beurteilung der Tragfähigkeit einer ToB unter Betondecken. Von den untersuchten Kiestragschichten wies eine modifizierte Kiestragschicht die beste Eignung für die Anwendung unter einer Betondecke auf. Das korngestufte Baustoffgemisch bestand aus gebrochener Gesteinskörnung <8 mm (Korngruppe 0/2 mm gewaschen) und ungebrochener Gesteinskörnung >8 mm, Erweiterung des Sieblinienbereichs von STSuB bei 2 mm von 28 auf 31 %, Feinanteil < 0,063 mm im eingebauten Zustand <5 Masse %, Wasserdurchlässigkeit in der Laborprüfung mit Durchlässigkeitsbeiwert k ≥ 5,4 • 10-5 m/sec. Eine theoretische Untersuchung zeigte, dass eine Reduzierung des EV2-Wertes einer ToB von 180 auf 150 N/mm2 unter Verkehrslast nur eine geringe Spannungserhöhung in der Betondecke herbeiführt. Bei modifizierten KTS mit einem entsprechend optimierten Anteil an gebrochener Gesteinskörnung kann auch bei Auflagerung auf einer Frostschutzschicht die Anforderung an den Verformungsmodul auf der Oberfläche der ToB mit EV2 ≥ 150 N/mm2 beibehalten werden. Gegen den Einsatz entsprechender ToB unter Betondecken bestehen keine Bedenken.
Die neuen TL/ZTV/TP Fug-StB
(2013)
Eine Betondecke kann nur so gut sein wie ihre Fugen und Fugenfüllsysteme. Funktionierende Fugen sind daher ein wesentlicher Bestandteil der Betonstraße. Nur mit funktionierendem Fugenfüllsystem kann die prognostizierte Lebensdauer einer Betondecke von mindestens 30 Jahren erreicht werden. In diesem Sinne wurden im Jahre 2001 die ZTV Fug-StB 01) eingeführt, um durch technische Vorgaben einen hohen Standard bei der Herstellung von Fugen zu gewährleisten. Aufgrund notwendiger Neuerungen, technischer Weiterentwicklung bei der Herstellung von Fugenmassen und -profilen sowie der Umsetzung der Europäischen Normen in das Deutsche Regelwerk war nach 10 Jahren nun eine Überarbeitung notwendig. Der Entwurf der neuen ZTV Fug-StB gliedert sich nach dem Kapitel "Allgemeines" in vier Teile für die unterschiedlichen Fugenfüllsysteme. Die neuen ZTV Fug-StB sind für Beton- und Asphaltflächen ebenso wie für Verkehrsflächen auf Bauwerken, Pflasterflächen, Schienenfugen und Riss-Sanierungen anwendbar. Es werden neu entwickelte Fugenkonstruktionen behandelt. Die Bedeutung funktionierender Fugen und Fugenfüllsysteme wird anhand aktueller Themen sehr deutlich. Derzeit werden verstärkt Schäden bei Fugen an neuen Betondecken, insbesondere Flankenablösungen und Versprödungen der Fugenvergussmasse beobachtet. Hier werden mögliche Schadensursachen ermittelt mit dem Ziel, über die komplexen Wirkungszusammenhänge ein Fugenfüllsystem mit Heißvergussmassen zu entwickeln, das den technischen Anforderungen an das Gesamtsystem "Betonstraße" gerecht wird.
Die guten Erfahrungen im Landesstraßennetz mit Decken aus Beton mit Fließmittel führten zu der Folgerung, die Eignung der überdeckten Fugen mit Querkraftübertragung auch für Decken aus Beton ohne Fließmittel und für höher belastete Straßen zu untersuchen. Dazu wurde eine Versuchsstrecke im Lastfahrstreifen der Autobahn A 9 und im Standstreifen der A 19 angelegt. Auswertungen ergaben, dass die Fuge mit voller Wirksamkeit hergestellt werden kann, jedoch gemessen an der Nutzungsdauer der Decke bei hoher Beanspruchung frühzeitig ihre Wirksamkeit verliert. Der Schwerverkehr wurde als ausschlaggebend für den Substanzverlust an den querkraftübertragenden Konsolen (Betondübeln) erkannt. Parallel mit dem Substanzverlust an den Betondübeln geht die Querkraftübertragung zur Nachbarplatte zurück. Der Einsatz der Fuge kann aufgund der Untersuchungsergebnisse für Fahrbahnen von höher belasteten Straßen nicht empfohlen werden. Sind die hohen Beanspruchungen weniger häufig und dynamisch, wie zum Beispiel auf Flächen für den ruhenden Verkehr, ist davon auszugehen, dass die Abnutzung der Betondübel geringer ausfällt und die Querkraftübertragung mit der Nutzungsdauer der Decke übereinstimmt. Für solche und ähnlich einzuordnende Straßentypen und Bauklassen empfiehlt es sich, die Fuge auf bewährte einfache Art und Weise in Betonen mit Fließmittel herzustellen.
Der gemeinsam vom Institut für Verkehrsplanung und Verkehrswegebau der Technischen Universität Berlin und von der Bundesanstalt für Straßenwesen, Köln, durchgeführte Forschungsauftrag des Bundesministers für Verkehr hatte zum Ziel, Lösungswege zu finden, wie der Betondecke - ohne die Zusammensetzung zu ändern - von Anfang an eine gute Griffigkeit mitgegeben werden kann. Hierzu wurden vier grundsätzliche Möglichkeiten der Oberflächenausführung in verschiedenen Varianten und auch Kombinationen systematisch im Hinblick auf Praktikabilität, Griffigkeit, Lärm, Ebenheit und Aufwand untersucht: 1. Strukturieren des Oberflächenmörtels (z.B. Rosshaarbesen, Stahlbesen nach TRRL) 2. Aufstreuen von gebrochenen Mineralstoffen auf den frischen Beton hinter dem Nachlaufglätter (z.B. Diabas 2/5 mit einer Gussasphalt-Riffelwalze angedrückt) 3. Einarbeiten von Brechsand in den Oberflächenmörtel durch den Nachlaufglätter (z.B. Siliziumkarbid 0,5/1) 4. Beseitigen des Oberflächenmörtels (in Anlehnung an die Waschbetontechnik) Die Untersuchungen erfolgten mit Unterstützung mehrerer Landesstraßenbauverwaltungen, die die umfangreichen Versuchsprogramme in anstehende Neubau- bzw. Erneuerungsprogramme für Autobahnen einbringen konnten. Insgesamt wurden auf sieben Versuchsstrecken etwa 100 Versuchsfelder angelegt, die in der Regel 50 m lang sind. Bei Abschluss des ersten Teils der Forschungsarbeit lagen die Betonfahrbahnen der Versuchsstrecken durchschnittlich etwa zwei Jahre unter Verkehr. Hinsichtlich ihres Griffigkeitsverhaltens kann allgemein festgestellt werden: - Eine stärkere Strukturierung der Feinmörtelschicht wirkt sich anfangs und längerfristig stets günstig auf den Kraftschluss zwischen Reifen und Fahrbahn bei Nässe aus. Die im "Merkblatt über Straßengriffigkeit und Verkehrssicherheit bei Nässe" genannten Richtwerte werden sicher erfüllt. - Technisch lassen sich derartige Oberflächen ohne zusätzlichen Mehraufwand mit Besen erzielen, deren Borsten relativ lang und steif sind. Die besten Ergebnisse wurden mit dem vom britischen Transport an Road Research Laboratory entwickelten Stahlbesen erzielt, gefolgt vom Kunststoffbesen nach Piassava-Art. - Die übrigen Verfahren, insbesondere das zusätzliche Anreichern der Feinmörtelschicht mit scharfen Mineralstoffen und das Beseitigen des Oberflächenmörtels in Anlehnung an die Waschbetontechnik, können das hohe Griffigkeitsniveau der mit dem englischen Stahlbesen strukturierten Oberflächen nur selten erreichen. Sie sind dabei wesentlich aufwendiger und meistens wenig praktikabel. Da die Anforderungen bezüglich Ebenheit ohne weiteres erfüllt wurden und auch die Lärmmessungen gegenüber den mit Rosshaarbesen behandelten Oberflächen keine signifikant höheren Werte ergaben, hat die abschließende Oberflächenstrukturierung frischer Betondecken mit dem englischen Stahlbesen bereits Eingang in die ZTV Beton 78 gefunden.
Es bestehen Möglichkeiten, die Griffigkeit von Betonfahrbahndecken durch besondere Ausbildung der Oberfläche zu beeinflussen, wie sich aus Untersuchungen der TH Berlin und der BASt mit dem standardisierten Messverfahren mit blockiertem Schlepprad (Stuttgarter Reibungsmesser) ergeben hat. Die in den Vorschriften für Betonfahrbahnen auf Straßen (Arbeitsanweisung 1939, TV Beton 72, ZTV Beton 78) enthaltenen Bestimmungen werden aufgeführt. Sie beruhen jeweils auf Ergebnissen von Versuchsstrecken mit verschiedenen Oberflächenausführungen: Strukturieren, Aufstreuen von gebrochenen Mineralstoffen, Einarbeiten von Brechsanden, Entfernen des Oberflächenmörtels. Bei Vergleichen der Wirkung des Abziehens mit Rosshaarbesen oder Stahlbesen hat sich der Stahlbesen als günstiger erwiesen. Weitere Versuche betreffen die Verbesserung alter Betondecken mittels Fräsen, zementgebundener Beschichtung mit Haftbrücken oder mit Reaktionsharzmörtel, bituminöser Beschichtung oder Oberflächenbehandlung. Eine künftige Erhöhung der Griffigkeit neuer Betondecken wird von einer Betonzusammensetzung mit rauhem und polierresistentem Sand erwartet.
Die klassische Bestimmung der Dicke des Straßenoberbaus in Deutschland ist eine auf Erfahrungswerten beruhende Kategorisierung der Verkehrswege in Straßenklassen mit standardisierten Aufbauten. Die rechnerische Dimensionierung für Straßen nach [RDO Beton 09] erlaubt es den bekannten, durch Erfahrungswerte belegten Bereich zu erweitern, sodass insbesondere für höhere Verkehrslasten und Sonderverkehrsflächen eine fundierte Dimensionierung des Oberbaus erfolgen kann. Die Berechnung der Lastzustände nach [RDO Beton 09] basiert auf den analytischen Lösungen von Differentialgleichungen. Dies erlaubt eine einfache und schnelle Berechnung der Belastungszustände der Betonplatten. Die Berechnung ist jedoch an Bedingungen gebunden, welche für die Lösung der Differentialgleichungen vorausgesetzt werden müssen. Damit liefern diese Gleichungen nur für einen begrenzten Parameterbereich exakte Ergebnisse. Um die Dimensionierung flexibel handhaben zu können, ist es notwendig, verschiedene Einflüsse pauschal über Anpassungsfaktoren zu berücksichtigen. Die Ergebnisse werden dadurch entsprechend unsicher. Das Berechnungsverfahren nach [RDO Beton 09] erlaubt in diesem Sinne nur eine pauschale Erfassung der Querkraftübertragung in den Fugen, der Vorverformung der Platte, der Lastverteilung im Plattenquerschnitt und des Einflusses mehrerer Radlasten. Auch bezüglich der Plattengeometrie und der detaillierten Erfassung der Einflussfaktoren sind dem Berechnungsmodell enge Grenzen gesetzt. Mit der Nutzung der Finite-Elemente-Methode ist es möglich, diese Defizite des Berechnungsmodells zu beseitigen. Die Dimensionierung wird damit genauer und flexibler. Die FEM bietet außerdem das Potenzial für eine wesentliche Weiterentwicklung des Dimensionierungsverfahrens. Im Rahmen des Forschungsvorhabens wurde ein Finite-Elemente-Modell definiert, welches geeignet ist, in einem Dimensionierungsprogramm nach [RDO Beton 09] die Grundlage für die Spannungsberechnung zu bilden. Das Modell umfasst 9 aus Volumenelementen modellierte Platten, einen Volumenblock für den Untergrund, sowie Anker und Dübel. Für die Berechnung des Modells wird das Programm CalculiX aus dem Open-Source-Bereich als Solver verwendet. Mithilfe von systematischen Serienrechnungen wurde das Modell optimiert und validiert. Um die Rechenzeit zu optimieren, wurde für die unterschiedlichen Berechnungsfälle geprüft, ob die Kalkulation der Spannungen an einem reduzierten Modell mit weniger Platten möglich ist. Die Einbindung in die Dimensionierungssoftware AWDSTAKO ermöglicht die FEM-basierte Dimensionierung nach [RDO Beton 09]. An ausgewählten Problemstellungen wurden die neuen Möglichkeiten, welche sich durch die FEM-Berechnung ergeben demonstriert.
Entwicklung eines scannenden Prüfgeräts zur Detektion von Delaminationen in Betonfahrbahndecken
(2019)
Ein bedeutender Teil (ca. 30 %) der Bundesautobahnen ist in Betonbauweise hergestellt. An solchen Fahrbahnen können spezielle Schadensbilder auftreten, die in Zusammenhang mit chemischen Reaktionen (insbesondere Schädigung aufgrund Alkali-Kieselsäure-Reaktion) oder mechanischer und thermischer Beanspruchung stehen (z. B. Hitzeschäden). Zur zerstörungsfreien Zustandserfassung im Hinblick auf substanzielle Schäden von Fahrbahndecken aus Beton steht derzeit noch kein wirtschaftlich sinnvoll einsetzbares Prüfsystem zur Verfügung, das als Entscheidungsgrundlage für Instandsetzungsmaßnahmen dienen könnte. Zwar gibt es Systeme mit denen z. B. die Tragfähigkeit oder der komplette Straßenaufbau (Georadar) repräsentativ und auch mit hohen Scangeschwindigkeiten abgebildet werden kann. Jedoch ist die Abbildung von auf der Oberfläche nicht sichtbaren horizontalen Rissen und Delaminationen im Inneren der Betondecke nur mit großem Aufwand messtechnisch durchführbar. Deshalb wurde im Rahmen des hier beschriebenen Forschungsvorhabens ein scannendes Messverfahren entwickelt und in einem Prototypensystem implementiert. Das System erlaubt die Durchführung von Messungen auf Basis von elastischen Wellen- und Schwingungsphänomenen, die direkt mit strukturellen Eigenschaften wie z. B. dem Vorhandensein von Rissen korrelierbar sind. Das entwickelte Messsystem nutzt als Grundlage das sog. Impakt-Echo-Verfahren, bei dem durch einen mechanischen Impakt elastische Wellen im Betonkörper ausgelöst, mit geeigneter Sensorik empfangen und mit Methoden der Datenverarbeitung im Hinblick auf Informationen bezüglich Materialkennwerten und Schäden analysiert werden. Im Laufe der Entwicklungsarbeiten wurden messtechnische Komponenten wie Sensorik, Signalquellen und Messelektronik für die speziellen Erfordernisse scannender Messungen an Betonfahrbahndeckenim Bestand konzeptioniert, hergestellt und optimiert. Insbesondere wurde zur Realisierung der scannenden Funktionsweise eine luftschallbasierte Signalaufzeichnung implementiert. Darüber hinaus wurden auf Basis numerischer Simulationen und Realmessungen Methoden zur Datenverarbeitung und korrekten Interpretation der Messdaten erarbeitet. Testmessungen wurden sowohl an ausgebauten Fahrbahnplatten als auch an ausgewählten Fahrbahnen im Bestand durchgeführt. Mit dem System konnten an Fahrbahnen unterschiedlicher Bauart Messergebnisse erzielt werden, die Rückschlüsse auf das Vorhandensein horizontaler Risse ermöglichen. Bei Vorliegen mehrerer Rissebenen ergibt sich durch das Messprinzip die Einschränkung, dass nur die oberste Rissebene detektierbar ist. Die Messergebnisse konnten an ausgewählten Stellen durch Kernbohrungen verifiziert werden. Wo keine direkte Verifikation möglich war, ergab sich eine gute Übereinstimmung mit alternativen Messverfahren (Ultraschall) oder eine plausible Übereinstimmung mit dem allgemeinen Fahrbahnzustand, der z. B. durch Ausbesserungsstellen im umgebenden Bereich der Messlokationen ersichtlich war. Das Prototypensystem erlaubt erstmals eine scannende Erfassung struktureller Schädigung durch horizontale Risse und Delaminationen in Betonfahrbahndecken von einer beweglichen Plattform aus. Obwohl noch Optimierungsmöglichkeiten v. a. hinsichtlich der Scangeschwindigkeit bestehen, ergab sich durch die Bearbeitung des Forschungsvorhabens eine wesentliche Verbesserung bestehender Prüftechnik zur Abbildung kleinskaliger Schäden in Fahrbahndecken aus Beton.
Gegenstand des Forschungsvorhabens war es, aus den Ergebnissen zerstörungsfrei arbeitender Messsysteme und erweiterten Informationen (z.B. Aufbau, Alter und Zustand der Strecken) eine Systematik zu entwickeln, mit der die Ermittlung von repräsentativen homogenen Abschnitten möglich ist. Auf vier ausgewählten Beton- und drei Asphaltabschnitten erfolgte die Analyse der ZEB-Daten und der nur lückenhaft vorliegenden Bestandsdaten. Parallel dazu erfolgten Messungen mit dem Georadar. Zur Verifizierung der ZEB-Ergebnisse und zur Interpretation der Ergebnisse der Georadarmessungen wurde zusätzlich eine Streckenbegehung mit visueller Zustandserfassung durchgeführt. Gleichzeitig konnten mit der visuellen Zustandserfassung in begrenztem Umfang fehlende Angaben zur Erhaltungsgeschichte der Fahrbahnen gesammelt werden. Anhand von Bohrkernentnahmen wurden Schichtaufbauten und Schichtdicken ermittelt, die einerseits dem Abgleich mit Bestandsdaten und andererseits zur Kalibrierung der Georadarmessungen dienten. Zu den relevanten Einzelmerkmalen hinsichtlich der strukturellen Substanz wurden homogene Abschnitte gebildet, die in einem weiteren Schritt zu übergeordneten homogenen Abschnitten zusammengefasst wurden. Zur Untersuchung dieser Abschnittsbildung wurden FWD-Messungen durchgeführt und die Abschnittsbildung aufgabenbezogen interpretiert. Aus zwei parallel dazu laufenden Forschungsarbeiten wurden die Ergebnisse von Laborversuchen aus den an diesen Strecken entnommenen Bohrkernen zur Untersuchung der übergeordneten Abschnitte hinzugezogen. Im Ergebnis kann festgestellt werden, dass eine Abschnittsbildung für eine spätere Bewertung der strukturellen Substanz prinzipiell erfolgen kann, wenn relevante ZEB-Daten mit einer visuellen Zustandserfassung präzisiert und mit qualitativ hochwertigen Georadardaten kombiniert werden. Letztere müssen momentan jedoch noch mit großem Aufwand ausgewertet werden. FWD-Daten waren bei den untersuchten Strecken als Ergänzung und Präzisierung nur in einigen Fällen sinnvoll. Bei Strecken mit relativ homogenen Randbedingungen und geringem Schädigungsgrad sind statistisch repräsentative Bohrkernentnahmen dennoch erforderlich, um Abschnittsgrenzen von Homogenbereichen zu detektieren, die dann nur noch von den mechanischen Kenngrößen des gebundenen Oberbaus abhängig sind.
Schäden an Betonfahrbahnen sind fast immer auf das Eindringen von Wasser unter die Betonplatte zurückzuführen. Für die Erprobung von Entwässerungseinrichtungen wurden Versuchsstrecken auf den Autobahnen A5 (Frankfurt -Mörfelden), A7 (bei Dorfmark und Soltau) sowie der A 29 (Bei Sage) eingerichtet, bei denen verschiedene Maßnahmen (Längsentwässerung, Punktentwässerung, Flachdrainage) auf ihr Verhalten beobachtet werden.
Während Betonfahrbahnen auch nach 10 Jahren unter Wetter- und Verkehrseinflüssen noch gute Oberflächeneigenschaften aufweisen, ist die Längsebenheit mancher schwerbelasteter Autobahnen weniger zufriedenstellend. Die Schäden sind fast immer auf das in die Straßenbefestigung eingedrungene Wasser zurückzuführen. Es wird über die Ergebnisse von Probestrecken zur Fernhaltung oder Ableitung des Wassers berichtet. Die Schäden entstehen durch das hydrodynamische Pumpen durch den Verkehr an undichten Fugen und Rissen mit der Folge von Erosion der Tragschicht. Verschiedentlich sind auch Schäden durch Frosthebungen entstanden, wenn die Durchlässigkeit der Frostschutzschicht geringer als 10 hoch -5 m/s ist. Für die Ableitung des Wassers gibt es drei Abflussebenen: Deckenoberfläche, Grenzschicht zwischen Decke und oberer Tragschicht und Erdplanum. Auch bei der einfachsten Lösung, Ableiten des Wassers über die Oberfläche, kann vollständiges Eindringen nicht verhindert werden. Bei wenig durchlässiger Tragschicht wird das Wasser durch eine flächige Drainage oder Längs- und Querdrainage abgeleitet. Vergleichende Versuche mit 50 m langen Probestrecken werden beschrieben. Hinsichtlich der Wirksamkeit ergibt sich folgende Reihenfolge: Längsentwässerung; Drainbeton, Dränasphalt und 10 mm dickes Geotextil; 3 bis 5 mm Geotextil, Punktdrainage mit Rohren; Flachdrain. Die Auswahl der aussichtsreichsten Maßnahme wird erörtert. Auf eine Dichtung der Fugen kann in keinem Fall verzichtet werden.